Yb-Er: Phosphate Glass Laser Rods (LD 930-970 nm pumping)


PARAMETER VALUE
 
  Wavelength   1.535 micron  
  Yb concentration by weight

Er concentration by weight
  15% (up to 30% upon request)

0.05% (up to 1.5% upon request)
 
  Flatness of plane surface   Lambda/10 at L=0.63 micron  
  Parallelism   20 arc seconds  
  Perpendicularity   5 arc minutes  
  Scratch - dig   20 - 10 (10 - 5 upon request)  
  Homogeneity of refractive index   ± 1 x 10-5  
  Reflectivity of AR coatings   Less than 0.25% at 1.535 micron  
  Damage threshold of AR coatings   1 GW/cm2  

Dimension, mm Part Number
 
  Dia. 1.0 - 10 x 2- 50.0   xxxxxxxxxx  

 



 
 
 
Nd: Phosphate Glass
Nd : YLF Laser Rods
Cr-Yb-Er: Phosphate Glass Laser Rods
Yb-Er: Phosphate Glass Laser Rods